Discovery Series Differential Scanning Calorimeter DSC

The Discovery DSC represents the latest innovation from TA Instruments. Building on the Tzero® technology, the Discovery DSC introduces innovative Diffusion-Bonded Sensor technology. The Discovery DSC provides unmatched precision, accuracy, industry-leading sensitivity and resolution. Tzero Technology provides the flattest baselines, and highest combined sensitivity and resolution of any DSC available. The Discovery DSC provides unmatched precision, repeatability and accuracy of heat flow and temperature measurements, while maintaining industry-leading sensitivity and resolution. The Discovery DSC delivers the highest sensitivity for a diverse range of heat flow transitions, across a wide range of experimental scanning rates. The result is the highest level of sensitivity for your materials, under any experimental condition.

equipment specifications
Temperature Range -180 –725 °C
Temperature Accuracy ±0.025 °C
Temperature Precision ±0.005 °C
Enthalpy Precision ±0.04%
Heat Flow Noise (rms) ≤0.08 μW
Baseline Linearity (-50°–400 °C) ≤5 μW
Baseline Accuracy(-50°–400 °C) ±20 μW
Baseline Repeatability (-50°–400 °C) ±5 μW
Direct CpAccuracy(-50°–400 °C) ≤3%
Direct CpPrecision (-50°–400 °C) ≤1%
Direct CpRepeatability (-50°–400 °C) ≤1%

sample size: 1 – 10 mg